Product Details:
Payment & Shipping Terms:
|
Formula: | LaAlO3 | Growth Method: | Cz Method |
---|---|---|---|
Color And Appearance: | From Brown To Brownish | Thermal Expansion: | 9.4x10-6/℃ |
Crystal Density: | 6.52g/cm³ | Hardness: | 6.5 Mohs |
Melting Point (℃): | 2080℃ | Permittivity: | ε = 21 |
High Light: | LaAlO3 Crystal Transparent,Low Dielectric Constant LaAlO3 Crystal,LaAlO3 Crystal Brown |
Size | Max Φ 76.2mm (3''inches) |
Thickness | 0.5mm /1.0 mm |
Polishing | Single or Double |
Crystal Orientation | <100> <110> <111> |
Redirection precision | ±0.5° |
Redirection the edge | 2°(special in 1°) |
Angle of crystalline | Special size and orientation are available upon request |
Ra | ≤5Å(5µm×5µm) |
Pack | Class100 clean bag,Class 1000 clean bag |
Contact Person: Zheng
Tel: +86 18255496761
Fax: 86-551-63840588
Dia 76mm Faraday Devices TGG Single Crystal Magneto Optical Crystals
Fiber Laser Faraday Isolator Crystal Magneto Optic TSAG Crystal
Faraday Rotator And Isolator TSAG Magneto Optical Crystals
Magneto Optical Crystals Terbium Scandium Aluminum Garnet TSAG Crystal Rods
Lutetium Alluminium Garnet Scintillation Crystals LED Lighting Ce LUAG Crystal
High Density Scintillating Material Lutetium Aluminum Garnet Ce LUAG Crystal
Scintilation Material Cerium Doped Lutetium Aluminium Garnet Ce LUAG Crystal